A galvanizing samar line ne cikakken sa na kayan aiki don zafi-tsoma galvanizing Layer na zinc gami shafi a bangarorin biyu na karfe nada.Ya ƙunshi na'ura mai ƙarewa, na'ura mai daidaita tashin hankali, injin mai, injin shear, injin iska da sauran kayan aiki.
Babban tsari kwarara na galvanized takardar

8-8-1

Coiling → Yanke wutsiya biyu → yankan kai da yankan wutsiya → walda → tsaftacewa alkaline → gogewa na farko → tsaftacewa ta lantarki → gogewa ta biyu → kurkurawar ruwan zafi → bushewar iska mai zafi → madaidaicin mashigar → ci gaba da sanyaya → zafi tsoma galvanizing ( yumbu zinc tukunya) → iska busa wuka (gabatarwa) → → sanyaya iska bayan plating → quenching water → leveling machine (ajiye) → mikewa → maganin wuce gona da iri (ajiye don juriya na yatsa)

Ayyukan kowane sashe na layin galvanizing

Sashin tsaftacewa: Cire sanyi mai birgima da foda na ƙarfe daga saman tsiri.Tsaftacewa kafin madauki na shigarwa yana sauƙaƙe bin diddigin tsiri a cikin madauki yayin da yake guje wa haƙora da tarkace.

Sashin madauki na shiga: Yana ba da madaidaicin madaidaicin tsayi mai tasiri lokacin da waldi ya tsaya a ƙofar, yana ba da damar ci gaba da samar da layin samarwa.

Sashin murhun wuta: murhun murɗawa mai ci gaba a tsaye, yana kaiwa ƙayyadadden zagayowar ɓarna.

Sashen Galvanizing: Ana tsoma tsiri a cikin tukunyar tutiya da aka narkar da don yin galvanizing.

Sassan mai daidaitawa da tashin hankali: ingantaccen aiki.

Sashen jiyya (passivation): Tandem twin roll coater tare da tanderun wuta da sanyaya don shafi farin tsatsa da resistant chromate mafita.

Sashin madauki: Lokacin da sashin fita ya daina yankewa, ana ba da madaidaicin madaidaicin tsayi mai tasiri don sa layin samarwa ya ci gaba da gudana.